Found results for
patents
1.
|
WELL SEALING MATERIAL AND METHOD OF PRODUCING A PLUG
| Application Number |
18199094 |
| Status |
Pending |
| Filing Date |
2023-05-18 |
| First Publication Date |
2023-09-14 |
| Owner |
Rawwater Engineering Limited (United Kingdom)
|
| Inventor |
- Eden, Robert
- Oluleke, Joseph
|
Abstract
Bismuth-based alloys comprising at least about 50% by weight bismuth, about 30 to about 35% by weight tin, and about 1.8 to about 2.8% by weight antimony; and an alloy of bismuth and silver comprising about 90 to about 97% by weight bismuth and about 3 to about 9% by weight silver. A plug comprising an alloy of bismuth, tin, and antimony; and a plug comprising an alloy of bismuth and silver. A method of using a plug made from a bismuth-based alloy to seal a well, wherein a length of a well is filled with the molten alloy and the molten alloy is allowed to solidify.
|
2.
|
METHOD OF REPAIRING A DEFECT AND DEVICE
| Application Number |
EP2022074896 |
| Publication Number |
2023/036839 |
| Status |
In Force |
| Filing Date |
2022-09-07 |
| Publication Date |
2023-03-16 |
| Owner |
RAWWATER ENGINEERING LIMITED (United Kingdom)
|
| Inventor |
Eden, Robert
|
Abstract
A method of and apparatus for repairing a defect in a surface are provided, the method comprising the steps of a) providing a bolus of an at least partially liquid alloy in a charge chamber, the charge chamber having a closable outlet and a closable pressure inlet; b) introducing a pressurized fluid to the charge chamber via the pressure inlet and accelerating the bolus such that the bolus is ejected from the charge chamber via the outlet; c) directing the bolus along a pathway between the charge chamber and the defect such that the bolus contacts the defect; and d) solidifying the at least partially liquid alloy while it is contact with the defect.
IPC Classes ?
- B22F 10/22 - Direct deposition of molten metal
- B23P 6/00 - Restoring or reconditioning objects
- C23C 4/06 - Metallic material
- C23C 4/08 - Metallic material containing only metal elements
- C23C 4/123 - Spraying molten metal
- B05C 11/10 - Storage, supply or control of liquid or other fluent materialRecovery of excess liquid or other fluent material
- B05B 12/06 - Arrangements for controlling deliveryArrangements for controlling the spray area for controlling time, or sequence, of delivery for effecting pulsating flow
|
3.
|
Well sealing material and method of producing a plug
| Application Number |
17254091 |
| Grant Number |
12000237 |
| Status |
In Force |
| Filing Date |
2019-06-21 |
| First Publication Date |
2021-08-26 |
| Grant Date |
2024-06-04 |
| Owner |
RAWWATER ENGINEERING LIMITED (United Kingdom)
|
| Inventor |
- Eden, Robert
- Oluleke, Joseph
|
Abstract
Bismuth-based alloys comprising at least about 50% by weight bismuth, about 30 to about 35% by weight tin, and about 1.8 to about 2.8% by weight antimony; and an alloy of bismuth and silver comprising about 90 to about 97% by weight bismuth and about 3 to about 9% by weight silver. A plug comprising an alloy of bismuth, tin, and antimony; and a plug comprising an alloy of bismuth and silver. A method of using a plug made from a bismuth-based alloy to seal a well, wherein a length of a well is filled with the molten alloy and the molten alloy is allowed to solidify.
|
4.
|
METHOD OF SEALING A SURFACE AND DEVICE THEREFOR
| Document Number |
03104763 |
| Status |
Pending |
| Filing Date |
2019-06-21 |
| Open to Public Date |
2020-01-02 |
| Owner |
RAWWATER ENGINEERING LIMITED (United Kingdom)
|
| Inventor |
Eden, Robert
|
Abstract
A method of sealing a surface is provided, the method comprising the steps of providing a metallic composition; providing a propellant; heating the metallic composition to above the melting point of the metallic composition to provide at least partially liquid metallic composition; accelerating the at least partially liquid metallic composition towards the surface by means of the propellant; and applying the at least partially liquid metallic composition to the surface.
IPC Classes ?
- C23C 4/06 - Metallic material
- C23C 4/08 - Metallic material containing only metal elements
- C23C 4/123 - Spraying molten metal
- G21F 1/00 - Shielding characterised by the composition of the material
|
5.
|
IMPROVED WELL SEALING MATERIALCOMPRISING AN ALLOY COMPOSITION OF BISMUTH, TIN, AND ANTIMONY ANDMETHOD OF PRODUCING A PLUG FOR SEALING A WELL
| Document Number |
03104767 |
| Status |
Pending |
| Filing Date |
2019-06-21 |
| Open to Public Date |
2020-01-02 |
| Owner |
RAWWATER ENGINEERING LIMITED (United Kingdom)
|
| Inventor |
- Eden, Robert
- Oluleke, Joseph
|
Abstract
Bismuth-based alloys and the use of plugs made from such alloys to seal wells as well as the plugs themselves are provided. There is provided an alloy of bismuth, tin, and antimony comprising at least about 50% by weight bismuth, about 30 to about 35% by weight tin, and about 1.8 to about 2.8% by weight antimony; and an alloy of bismuth and silver comprising about 91 to about 97% by weight bismuth and about 3 to about 9% by weight silver. There is also provided a method for producing a plug comprising an alloy of bismuth, tin, and antimony; and a method for producing a plug comprising an alloy of bismuth and silver; wherein a length of a well is filled with the molten alloy and the molten alloy is allowed to solidify.
|
6.
|
METHOD OF SEALING A SURFACE AND DEVICE THEREFOR
| Application Number |
GB2019051752 |
| Publication Number |
2020/002886 |
| Status |
In Force |
| Filing Date |
2019-06-21 |
| Publication Date |
2020-01-02 |
| Owner |
RAWWATER ENGINEERING LIMITED (United Kingdom)
|
| Inventor |
Eden, Robert
|
Abstract
A method of sealing a surface is provided, the method comprising the steps of providing a metallic composition; providing a propellant; heating the metallic composition to above the melting point of the metallic composition to provide at least partially liquid metallic composition; accelerating the at least partially liquid metallic composition towards the surface by means of the propellant; and applying the at least partially liquid metallic composition to the surface.
IPC Classes ?
- C23C 4/06 - Metallic material
- C23C 4/08 - Metallic material containing only metal elements
- C23C 4/123 - Spraying molten metal
- G21F 1/00 - Shielding characterised by the composition of the material
|
7.
|
IMPROVED WELL SEALING MATERIAL AND METHOD OF PRODUCING A PLUG
| Application Number |
GB2019051755 |
| Publication Number |
2020/002887 |
| Status |
In Force |
| Filing Date |
2019-06-21 |
| Publication Date |
2020-01-02 |
| Owner |
RAWWATER ENGINEERING LIMITED (United Kingdom)
|
| Inventor |
- Eden, Robert
- Oluleke, Joseph
|
Abstract
Bismuth-based alloys and the use of plugs made from such alloys to seal wells as well as the plugs themselves are provided. There is provided an alloy of bismuth, tin, and antimony comprising at least about 50% by weight bismuth, about 30 to about 35% by weight tin, and about 1.8 to about 2.8% by weight antimony; and an alloy of bismuth and silver comprising about 91 to about 97% by weight bismuth and about 3 to about 9% by weight silver. There is also provided a method for producing a plug comprising an alloy of bismuth, tin, and antimony; and a method for producing a plug comprising an alloy of bismuth and silver; wherein a length of a well is filled with the molten alloy and the molten alloy is allowed to solidify.
|
|