NODULARIZATION METHOD FOR NODULAR CAST IRON
Numéro d'application |
CN2013001050 |
Numéro de publication |
2014/134762 |
Statut |
Délivré - en vigueur |
Date de dépôt |
2013-09-06 |
Date de publication |
2014-09-12 |
Propriétaire |
TIANJIN WANLU LIMITED COMPANY OF SCIENCE AND TECHNOLOGY (Chine)
|
Inventeur(s) |
- Liu, Nianlu
- Liu, Changchen
|
Abrégé
A nodularization method for nodular cast iron, comprising: masoning a left vertical-surface baffle (2) and a right vertical-surface baffle (3) at the bottom of a nodularization ladle (1); a semicircular upper cover plate (4) of a reaction chamber is horizontally masoned on the top of the left vertical-surface baffle (2) and the right vertical-surface baffle (3); the vertical surface of the reaction chamber is provided with one or more reaction chamber feed inlets (5) thereon; the upper end of one of the reaction chamber feed inlets (5) is provided with a pressure-relief groove (6); the upper end of the pressure-relief groove (6) is flush with the semicircular upper cover plate (4) of the reaction chamber; the masoned nodularization ladle is dried for subsequent nodularization. Nodularization comprises the following steps: placing the desired weight of integral rare earth magnesium ferrosilicon nodulizer (8), low-silicon nodulizer or non-silicon nodulizer without being externally lined with steel pipe into the reaction chamber of the nodularization ladle (1); placing the ferrosilicon inoculants into the reaction chamber of the nodularization ladle (1), the ferrosilicon inoculants being piled at the reaction chamber feed inlet (5); the molten iron is poured into the nodularization ladle (1) to conduct nodularization reaction; cleaning the scum after the nodularization reaction, and adding the composite inoculants to cover the molten iron.
Classes IPC ?
- C21C 1/10 - Fabrication des fontes à graphite sphéroïdal
- B22D 1/00 - Traitement des métaux en fusion dans la poche ou dans les chenaux de coulée avant le moulage
|
2.
|
NODULARIZATION-PROCESSING METHOD
Numéro d'application |
CN2012000861 |
Numéro de publication |
2013/188993 |
Statut |
Délivré - en vigueur |
Date de dépôt |
2012-06-21 |
Date de publication |
2013-12-27 |
Propriétaire |
TIANJIN WANLU LIMITED COMPANY OF SCIENCE AND TECHNOLOGY (Chine)
|
Inventeur(s) |
- Liu, Nianlu
- Liu, Changchen
|
Abrégé
Provided is a nodularization-processing method for producing nodular cast iron. The method comprises: pouring a melted rare earth ferrosiliconmagnesium nodularizer alloy liquid containing Mg ≤20%, Si≤65%, and RE≤3% into a square steel tube for solidification and cooling; fixing the whole rare earth ferrosiliconmagnesium nodularizer lined on the outside with the square steel tube into a nodularization ladle using the inner and bottom masonry refractory bricks and wedge chocks in the nodularization ladle covered with a ladle cover, nodularization-processing through a pour-over ladle method; controlling the time for the nodularization reaction accurately, the temperature reduction of the molten iron being small during the nodularization-processing and pouring, the absorption rates of Mg, RE and Si becoming high after the nodularization-processing; 15 minutes after the completion of the nodularization reaction no decline in spheroidization occurs, thus improving the production environment during the manufacturing of a nodularizer and use thereof and significantly reducing production costs and increasing the quality of the product. Compared with a traditional rare earth ferrosiliconmagnesium nodularizer containing RE at a content of 2-8%, the nodularization-processing by the above method realizes the reduction of the usage amount of RE by 50-75%.
Classes IPC ?
- C22C 33/10 - Fabrication de fontes alliées comportant des procédés pour ajouter du magnésium
|
3.
|
SMOKELESS SPHEROIDIZATION PROCESSING METHOD
Numéro d'application |
CN2011001762 |
Numéro de publication |
2012/106837 |
Statut |
Délivré - en vigueur |
Date de dépôt |
2011-10-24 |
Date de publication |
2012-08-16 |
Propriétaire |
TIANJIN WANLU LIMITED COMPANY OF SCIENCE AND TECHNOLOGY (Chine)
|
Inventeur(s) |
- Liu, Nianlu
- Liu, Changchen
|
Abrégé
A smokeless spheroidization processing method for producing nodular cast iron. Disposed in the center of a side of a rectangular or square steel pipe (13) are multiple pressure-adjusting throughholes (17) or a pressure-adjusting slit (19). Melted alloy liquid of a nodulizer of rare earth, magnesium, silicon, and iron (18) comprising Mg ≤ 20%, Si ≤ 65% and RE ≤ 3% is injected into the steel pipe (13) for solidification and cooling; a rod having a pressing head (1) fixes the nodulizer of rare earth, magnesium, silicon, and iron (18), encased in the rectangular or square steel pipe (13), inside of a spheroidization ladle (7); the rod having a pressing head (1) has a weight iron and is hung by a hook (16) of an electric motor-powered hoisting device, or the rod having a pressing head (1) is connected by a first bolt (8) on a steering shaft (2), the steering shaft (2) being disposed on a lever (4) that pivots on a lever pivot shaft, the lever pivot shaft being a third bolt and nut (12) disposed on an upright post and position-fixing and measuring scale (6). Ladle-flushing method is adopted to precisely control the spheroidization reaction time and to enable smokeless spheroidization. The absorption rates of Mg, RE, and Si are high after the reaction, thereby improving the manufacturing environment of the nodulizer preparation process and application process, and reducing production costs while enhancing product quality.
Classes IPC ?
- C22C 33/10 - Fabrication de fontes alliées comportant des procédés pour ajouter du magnésium
- C21C 7/00 - Traitement à l'état liquide des alliages ferreux, p. ex. des aciers, non couverts par les groupes
|
4.
|
WATER-SAVING CLOSET AND WATER-SAVING URINAL FOR MALE
Numéro d'application |
CN2011000319 |
Numéro de publication |
2011/120326 |
Statut |
Délivré - en vigueur |
Date de dépôt |
2011-02-28 |
Date de publication |
2011-10-06 |
Propriétaire |
TIANJIN WANLU LIMITED COMPANY OF SCIENCE AND TECHNOLOGY (Chine)
|
Inventeur(s) |
Liu, Nianlu
|
Abrégé
A water-saving closet comprises a bowl (1), a funnel (2), a floating ball and a pulling wire (3), a water sealing structure, a seat cushion (6), an upper cover (8), a plactic shielding cover (15) et al. The water seal structure comprises an inner water seal tank (11), an outer water seal tank (12), a rotary tank inside the inner water seal tank (11) and a rotary tank outside of the outer water seal tank (12). The closet can save water and prevent odor by using the water seal function of the floating ball and the water sealing structure. Furthermore a water-saving urinal for male comprises a bottle (18) for storaging urina, a funnel (20) with a water seal tank, a floating ball, a pulling wire and a pulling ring (21), an upper cover (23) of the bottle (18) for storaging urina et al. The urinal can save water and prevent odor by using the water seal function of the floating ball and the water seal structure.
Classes IPC ?
- A47K 11/00 - Cabinets sans chasse d'eauUrinoirs sans chasse d'eauPots de chambreChaises avec vase de toilette ou spécialement adaptées pour être utilisées avec une cuvette de toilette
- A47K 11/02 - Cabinets fonctionnant à sec, p. ex. cabinets avec incinération
- A47K 11/04 - Cuvettes de cabinets de chambreChaises avec vase de toilette ou spécialement adaptées pour être utilisées avec une cuvette de toilette, p. ex. chaises percées
- A47K 11/12 - Urinoirs sans chasse d'eau
- A47K 13/00 - Sièges ou couvercles pour toutes sortes de cuvettes de cabinets
- A47K 13/02 - Sièges ou couvercles pour toutes sortes de cuvettes de cabinets en matière plastique
- A47K 13/26 - Dispositifs de montage pour sièges ou couvercles
|
5.
|
OIL SMOKE PREVENTING COOKER
Numéro d'application |
CN2009001385 |
Numéro de publication |
2010/075666 |
Statut |
Délivré - en vigueur |
Date de dépôt |
2009-12-07 |
Date de publication |
2010-07-08 |
Propriétaire |
TIANJIN WANLU LIMITED COMPANY OF SCIENCE AND TECHNOLOGY (Chine)
|
Inventeur(s) |
Liu, Nianlu
|
Abrégé
An oil smoke preventing cooker that is composed of a frying pan body (1) and an oil smoke preventing metal ring (2) is provided. The inside profile of the frying pan body (1) is circular arc, or the pan brim is circular arc and the pan bottom is flat-bottomed. The wall thickness from the central position on the pan bottom whose diameter is 90-130 mm to the outer part of the pan body (1) whose diameter is 215 mm is 0.2-2.4 mm thicker than the wall thickness at central position on the pan bottom. The thickened part protrudes at outside of the frying pan body (1). The thickness of the center position of the frying pan bottom and the thickness from an upper edge of the frying pan to a position above the protruding thickened part are 1.0-2.5 mm. The oil smoke preventing cooker can control the rate of temperature rise of oil, increase quick-frying effect, and avoid the generation of the oil smoke.
Classes IPC ?
- A47J 27/00 - Récipients de cuisson
- A47J 36/00 - Éléments, détails ou accessoires des récipients de cuisson
- A47J 37/00 - Cuisson au fourRôtissageCuisson au grilFriture
|
|