Japan Prolong Limited Company

Japon

Retour au propriétaire

1-2 de 2 pour Japan Prolong Limited Company Trier par
Recheche Texte
Affiner par
Classe IPC
C04B 41/68 - Acide siliciqueSilicates 2
E04G 23/02 - Réparation, p. ex. comblement des lézardesRestaurationModificationAgrandissement 2
Résultats pour  brevets

1.

CONCRETE REPAIRING METHOD AND REPAIRING AGENT

      
Numéro d'application JP2018024530
Numéro de publication 2020/003430
Statut Délivré - en vigueur
Date de dépôt 2018-06-28
Date de publication 2020-01-02
Propriétaire JAPAN PROLONG LIMITED COMPANY (Japon)
Inventeur(s) Tomita Yutaka

Abrégé

Provided is a repairing method that enables filling a crack with gel so as to provide adequate water proofing properties and adequate water sealing properties even in the case where the width of the crack is equal to or greater than a certain width. The method comprises: a first step for injecting, spraying, or applying a silicate-containing solution to a concrete surface having a crack; a second step for performing filling by injecting or applying an inorganic material fluidized by addition of water, into the crack having the concrete surface moistened with the silicate-containing solution; and a third step for spraying or applying a silicate-containing solution to the concrete surface in which the crack has been filled with the inorganic material.

Classes IPC  ?

  • E04G 23/02 - Réparation, p. ex. comblement des lézardesRestaurationModificationAgrandissement
  • C04B 41/68 - Acide siliciqueSilicates

2.

CONCRETE REFORMING METHOD AND REFORMING MATERIAL

      
Numéro d'application JP2019025287
Numéro de publication 2020/004434
Statut Délivré - en vigueur
Date de dépôt 2019-06-26
Date de publication 2020-01-02
Propriétaire JAPAN PROLONG LIMITED COMPANY (Japon)
Inventeur(s) Tomita Yutaka

Abrégé

Provided is a reforming method that enables filling a crack with gel so as to provide adequate water proofing properties and adequate water-sealing properties even in the case where the width of the crack is equal to or greater than a certain width. The method comprises: a first step for injecting, spraying, or applying a silicate-containing solution to a concrete surface having a crack; a second step for performing filling by injecting or applying an inorganic material fluidized by addition of water, into the crack having the concrete surface moistened with the silicate-containing solution; and a third step for spraying or applying a silicate-containing solution to the concrete surface in which the crack has been filled with the inorganic material.

Classes IPC  ?

  • E04G 23/02 - Réparation, p. ex. comblement des lézardesRestaurationModificationAgrandissement
  • C04B 41/68 - Acide siliciqueSilicates